Skip to the guide

Power connections

Raychem BBIT at 105°C or 125°C

Copy 105°C from Storm's heat-shrink table and from Raychem sheet EPP 0607 1/08. Copy 125°C minimum from TE sheet EPP-0607-08/19.

Rust Belt Industrials · November 11, 2026 · 6 min read

On this page

Copy 105°C when the BBIT line follows Storm's heat-shrink table or the Raychem sheet Storm hosts. As of November 11, 2026, Storm's table lists Raychem BBIT at 35/36 kV with thermal endurance 105°C, and the hosted sheet, footer EPP 0607 1/08, prints thermal endurance 105°C minimum to IEC 216. Copy 125°C minimum when the line follows TE sheet EPP-0607-08/19. That sheet, opened the same day, prints thermal endurance 125°C minimum to IEC 216, and its title is voltage class 36 kV for application diameters 11 mm to 125 mm. Copy the cell from the document the drawing cites. The voltage row for the rest of Storm's tubing is on the heat-shrink page. Phase clearance for BBIT and BPTM is on the clearance page.

The 1/08 sheet matches Storm's 105°C cell. The 08/19 sheet prints 125°C

Storm's heat-shrink page, opened November 11, 2026, still pairs BBIT with voltage class 35/36 kV and thermal endurance 105°C. The link on the BBIT name opens a Raychem PDF whose footer is EPP 0607 1/08 and whose copyright line is Tyco Electronics. That PDF's key-product table prints thermal endurance to IEC 216 as 105°C minimum. Accelerated ageing on that sheet is 168 hours at 120°C, with tensile strength 10 MPa minimum and ultimate elongation 300 percent minimum. TE's later file, EPP-0607-08/19, prints thermal endurance to IEC 216 as 125°C minimum. Accelerated ageing on that sheet is 168 hours at 150°C, with the same 10 MPa and 300 percent minimums. A drawing that cites Storm's table, or the 1/08 PDF Storm links, uses 105°C. A drawing that cites EPP-0607-08/19 uses 125°C minimum.

BBIT thermal cells opened November 11, 2026. Voltage class on each document is 36 kV, or 35/36 kV on Storm's table.
DocumentThermal enduranceAccelerated ageingRecovered wall
Storm heat-shrink table105°CNot printed on the tableNot printed on the table
EPP 0607 1/08, hosted by Storm105°C minimum, IEC 216168 hours at 120°C. 10 MPa minimum. 300 percent minimum elongation.3.6 mm minimum on each size row. As-supplied wall 1.6 mm nominal.
EPP-0607-08/19125°C minimum, IEC 216168 hours at 150°C. 10 MPa minimum. 300 percent minimum elongation.3.6 mm minimum on each size row. As-supplied wall 1.6 mm nominal.

Both Raychem sheets keep the 36 kV title and the 3.6 mm wall

EPP 0607 1/08 says BBIT provides flashover protection up to 36 kV and is for circular and rectangular copper or aluminum busbars. The selection block says BBIT 25/10 fits rectangular bars from 17 mm to 28 mm and round bars from 11 mm to 20 mm, and BBIT 175/80 fits rectangular bars from 133 mm to 196 mm and round bars from 85 mm to 125 mm. Ordering rows print inside diameter as supplied and after recovery, a nominal wall of 1.6 mm as supplied, and a minimum wall of 3.6 mm after recovery. Roll lengths on that sheet are 25 m, 20 m, 15 m, 15 m, 15 m, and 10 m for the six sizes from BBIT-25/10-A/U-4 through BBIT-175/80-A/U-4. The note says to fit the larger size if two sizes fit, and it limits longitudinal change after free recovery to plus or minus 5 percent.

EPP-0607-08/19 uses the same six ordering descriptions and the same 1.6 mm nominal and 3.6 mm minimum wall on the rows that extracted with those headings. Its title is voltage class 36 kV, application diameter 11 mm to 125 mm. Dielectric strength on that sheet includes 350 kV/cm minimum at 1.00 mm, 180 kV/cm minimum at 2.00 mm, 150 kV/cm minimum at 2.50 mm, and 120 kV/cm minimum at 3.00 mm. The 1/08 sheet prints the 2 mm, 2.5 mm, and 3 mm dielectric lines at 180, 150, and 120 kV/cm minimum, and it does not print the 350 kV/cm line. Low-temperature flexibility on the 1/08 sheet is no cracking after 4 hours at -40°C. Flammability on that sheet is ANSI C37.20 and IEEE-27, no flame conveyance, 60 seconds maximum. The 1/08 clearance table for round busbars at 36 kV is 100 mm phase to phase and 160 mm phase to ground, against an IEC 71-2 air clearance of 320 mm. Rectangular busbars at 36 kV on that sheet are 140 mm phase to phase and 190 mm phase to ground, against the same 320 mm air clearance. The sheet says those clearances should not be adopted without testing by the user.

Storm's table is the 105°C cell next to 35/36 kV

On the Storm page opened November 11, 2026, BBIT is the red row at 35/36 kV, thermal endurance 105°C, flammability ANSI C37.20 and IEEE-27. BPTM on the same table is 25 kV and 125°C. The 125°C cell on Storm's table is the BPTM row. It is not a second BBIT cell. 3M BBI-A on that table is 5, 8, 15, 25, and 35 kV at 110°C. A bar whose drawing names BBIT and cites Storm's table stays on the 105°C cell. A bar whose drawing names the 08/19 TE sheet stays on 125°C minimum. The epoxy and BBIT page uses the tubing's 36 kV title and the size range. This page is the thermal cell that goes with the sheet the order names.

What to copy onto the BBIT line

  • Document: Storm's heat-shrink table, EPP 0607 1/08, or EPP-0607-08/19, as opened November 11, 2026.
  • Storm table: BBIT, 35/36 kV, 105°C, red, ANSI C37.20 and IEEE-27.
  • EPP 0607 1/08: 105°C minimum to IEC 216, ageing 168 hours at 120°C.
  • EPP-0607-08/19: 125°C minimum to IEC 216, ageing 168 hours at 150°C.
  • Wall, on either Raychem sheet: 1.6 mm nominal as supplied, 3.6 mm minimum after recovery.
  • Size: the BBIT row whose rectangular or round range covers the bar, from 11 mm round on the small size to 125 mm round on BBIT 175/80.
  • Clearance from EPP 0607 1/08 at 36 kV: 100 mm phase to phase and 160 mm phase to ground on a round bar, or 140 mm and 190 mm on a rectangular bar, and the sheet says the user tests before adopting them.

BBIT temperature note

Name the Raychem sheet or the Storm table. Copy that document's thermal endurance.

This prepares a request. It does not send one.

Questions the three BBIT documents answer

Which opened page prints 105°C for BBIT?

Storm's table and EPP 0607 1/08, as of November 11, 2026. The table cell is 105°C. The 1/08 sheet says 105°C minimum to IEC 216.

Which opened page prints 125°C for BBIT?

EPP-0607-08/19 prints 125°C minimum to IEC 216, as of November 11, 2026. Storm's 125°C cell is the BPTM row at 25 kV, not the BBIT row.

Did the ageing temperature move with the thermal cell?

The 1/08 sheet ages the tube for 168 hours at 120°C. The 08/19 sheet ages it for 168 hours at 150°C. Both still require 10 MPa minimum tensile strength and 300 percent minimum elongation after that ageing.

Sources

Storm's 35/36 kV and 105°C cells are from the heat-shrink page. The 105°C minimum, the 120°C ageing, the 3.6 mm wall, and the 36 kV clearances quoted above are from EPP 0607 1/08. The 125°C minimum and the 150°C ageing are from EPP-0607-08/19. All three were opened November 11, 2026.